Worked example
Example: Illustrative PC hook: 15 x 1.5 x 6 mm, 2 % strain, 1 mm undercut, 30 deg, mu 0.5. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Arm length | 15.000 mm |
| Arm thickness at the root | 1.5000 mm |
| Arm width | 6.0000 mm |
| Permissible strain (once or repeated) | 2.0000 % |
| Secant modulus at that strain | 2.0000 GPa |
| Coefficient of friction | 0.50000 - |
| Lead-in (mating) angle | 30.000 ° |
| Undercut (actual deflection) | 1.0000 mm |
Applying the formula below gives:
| Result | Value |
|---|---|
| Allowable deflection 0.67 ε l²/h | 2.0000 mm |
| Deflection force at the undercut | 3.0000 N |
| Mating (push-in) force | 4.5437 N |
| Strain at the actual undercut | 1.0000 % |
| Use of the allowable deflection | 0.50000 |
Open this example in the calculator and change any input.
Formula
\(y_{allow} = 0.67\frac{\varepsilon l^2}{h}, \quad P = \frac{bh^2}{6}\frac{E_s\varepsilon}{l}, \quad W = P\frac{\mu + \tan\alpha}{1 - \mu\tan\alpha}\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(l\) | Arm length | m |
| \(h\) | Arm thickness at the root | m |
| \(b\) | Arm width | m |
| \(\varepsilon\) | Permissible strain (once or repeated) | - |
| \(E_s\) | Secant modulus at that strain | Pa |
| \(\mu\) | Coefficient of friction | - |
| \(\alpha\) | Lead-in (mating) angle | rad |
| \(y\) | Undercut (actual deflection) | m |
| \(y_{allow}\) | Allowable deflection 0.67 ε l²/h | m |
| \(P\) | Deflection force at the undercut | N |
| \(W\) | Mating (push-in) force | N |
| \(\varepsilon_y\) | Strain at the actual undercut | - |
| \(y/y_{allow}\) | Use of the allowable deflection | - |
Method and standards
Beam theory for snap fits.
Where it is used
- Plastic housings, battery covers and clips.
- Design reviews of moulded assemblies.
Common mistakes
- Using the initial modulus instead of the secant modulus.
- Forgetting the root radius, which concentrates strain.
Assumptions and limits
- Rectangular constant section, small deflections, rigid mating part.
References
- Cantilever beam snap-fit design
Questions and answers
What strain can a snap fit take?
For a single assembly roughly 70 % of the strain at yield (often 2–6 % for unfilled thermoplastics, 1–2 % for glass-filled); about 60 % of that for repeated use.
How do I reduce the push-in force?
Use a shallower lead-in angle, a longer or thinner arm, or a tapered arm; the retention side can use a steep angle to resist pull-out.
What do the defaults represent?
An illustrative polycarbonate hook 15 mm long, 1.5 mm thick and 6 mm wide, 2 % permissible strain, 1 mm undercut, 30° lead-in and μ = 0.5.
Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.
Sources
Bayer MaterialScience, Snap-Fit Joints for Plastics: A Design Guide (2013), ch. 2, Budynas and Nisbett, Shigley's Mechanical Engineering Design, 9th ed. (McGraw-Hill, 2011), ch. 4