Worked example
Example: 200 HB normalised steel. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Brinell hardness | 200.00 - |
| Strength factor (MPa per HB) | 3.4500 - |
Applying the formula below gives:
| Result | Value |
|---|---|
| Estimated tensile strength | 690.00 MPa |
| Estimated endurance limit | 345.00 MPa |
Open this example in the calculator and change any input.
Formula
\(S_u \approx 3.45\,HB\ \mathrm{MPa}, \quad S_e' = \min(0.5S_u, 700\ \mathrm{MPa})\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(HB\) | Brinell hardness | - |
| \(k\) | Strength factor (MPa per HB) | - |
| \(S_u\) | Estimated tensile strength | Pa |
| \(S_e'\) | Estimated endurance limit | Pa |
Method and standards
Empirical correlations.
Where it is used
- Checking material in service by portable hardness.
- Screening fatigue strength.
Common mistakes
- Applying the rule to cast iron.
- Using the endurance limit without surface factors.
Assumptions and limits
- Steels (carbon and low-alloy). Above about 450 HB the relation is less reliable and is flagged.
References
- S_u ≈ 3.45 HB MPa (steels; Shigley's Mechanical Engineering Design, ch. 2) and S_e' = 0.5S_u up to 700 MPa (ch. 6)
Questions and answers
How accurate is the hardness rule?
About ±10 % for plain carbon and low-alloy steels; check with a tensile test for design.
Why cap the endurance limit at 700 MPa?
Above about 1,400 MPa tensile strength, fatigue strength stops rising in proportion.
What do the defaults represent?
A normalised medium-carbon steel at 200 HB.
Method and article reviewed by FireCAD engineering on 13 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.