Worked example
Example: Illustrative steel in still aerated water. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Diffusivity of the reactant | 2.0000e-05 cm²/s |
| Bulk concentration of the reactant | 0.26000 mmol/L |
| Electrons per reactant molecule (O₂: 4) | 4.0000 - |
| Diffusion boundary layer thickness | 0.50000 mm |
| Corroding metal molar mass | 55.845 kg/kmol |
| Metal valence | 2.0000 - |
| Metal density | 7,870.0 kg/m³ |
Applying the formula below gives:
| Result | Value |
|---|---|
| Limiting current density | 0.40138 A/m² |
| Equivalent uniform corrosion rate | 0.46578 mm/a |
| Mass loss rate | 10.036 g/(m²·d) |
Open this example in the calculator and change any input.
Formula
\(i_L = \frac{nFDC_B}{\delta}, \quad CR = \frac{i_LM}{zF\rho}\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(D\) | Diffusivity of the reactant | m²/s |
| \(C_B\) | Bulk concentration of the reactant | mol/m³ |
| \(n\) | Electrons per reactant molecule (O₂: 4) | - |
| \(\delta\) | Diffusion boundary layer thickness | m |
| \(M\) | Corroding metal molar mass | kg/kmol |
| \(z\) | Metal valence | - |
| \(\rho\) | Metal density | kg/m³ |
| \(i_L\) | Limiting current density | A/m² |
| \(CR\) | Equivalent uniform corrosion rate | m/s |
| \(\dot m''\) | Mass loss rate | kg/(m²·s) |
Method and standards
Limiting current.
Where it is used
- Corrosion in cooling and process water.
- Effect of flow and deaeration.
Common mistakes
- Using mg/L of oxygen as mol/m³.
- Ignoring flow effects on δ.
Assumptions and limits
- Diffusion-controlled cathode; uniform corrosion.
References
- Concentration polarisation and diffusion control
Questions and answers
Why does flow increase corrosion in neutral water?
It thins the diffusion layer, letting oxygen reach the surface faster.
How does deaeration help boilers?
Removing oxygen removes the cathodic reactant, cutting the limiting current and the corrosion rate.
What do the defaults represent?
Steel in air-saturated still water: O₂ at 0.26 mol/m³, D 2 × 10⁻⁹ m²/s, 0.5 mm boundary layer.
Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.
Sources
Fontana, Corrosion Engineering, 3rd ed. (McGraw-Hill, 1986)