Worked example
Example: 90 mm drum at 100 °C/h. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Wall thickness | 90.000 mm |
| Heating rate of the inner surface | 100.00 °C/h |
| Steel thermal conductivity | 45.000 W/(m·K) |
| Steel density | 7,850.0 kg/m³ |
| Steel specific heat | 0.50000 kJ/(kg·K) |
| Young's modulus | 200.00 GPa |
| Linear expansion coefficient | 13.000 µm/(m·K) |
| Poisson's ratio | 0.30000 - |
| Allowed through-wall ΔT | 40.000 K |
Applying the formula below gives:
| Result | Value |
|---|---|
| Thermal diffusivity | 11.465 mm²/s |
| Through-wall temperature difference | 9.8125 K |
| Surface thermal stress (magnitude; compressive at the inner surface while heating) | 24.298 MPa |
| Heating rate for the allowed ΔT | 407.64 °C/h |
Open this example in the calculator and change any input.
Formula
\(\alpha = \frac{k}{\rho c_p}, \quad \Delta T = \frac{\dot T s^2}{2\alpha}, \quad \sigma = \frac{E \beta}{1 - \nu}\cdot\frac{2}{3}\Delta T, \quad \dot T_{allow} = \frac{2\alpha\,\Delta T_{allow}}{s^2}\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(s\) | Wall thickness | m |
| \(\dot T\) | Heating rate of the inner surface | K/s |
| \(k\) | Steel thermal conductivity | W/(m·K) |
| \(\rho\) | Steel density | kg/m³ |
| \(c_p\) | Steel specific heat | J/(kg·K) |
| \(E\) | Young's modulus | Pa |
| \(\beta\) | Linear expansion coefficient | 1/K |
| \(\nu\) | Poisson's ratio | - |
| \(\Delta T_{allow}\) | Allowed through-wall ΔT | K |
| \(\alpha\) | Thermal diffusivity | m²/s |
| \(\Delta T\) | Through-wall temperature difference | K |
| \(\sigma\) | Surface thermal stress | Pa |
| \(\dot T_{allow}\) | Heating rate for the allowed ΔT | K/s |
Method and standards
One-dimensional heat conduction in a plane wall heated at a constant rate on the inside with the outside insulated: after the initial transient the temperature profile is a parabola that moves with the ramp (Carslaw and Jaeger). The surface stress follows from the difference between the mean and surface temperatures for a wall restrained against bending (Timoshenko). EN 12952-3 and similar codes set the actual start-up limits from pressure and thermal stress together with fatigue; they are not applied here.
Where it is used
- Start-up procedures.
- Cycling studies.
Common mistakes
- Using outer-surface rates.
Assumptions and limits
- Plane wall; constant properties. Drum curvature (thick cylinder) and the initial transient are neglected.
- Stress concentrations at nozzles and tube holes, which usually govern drum start-up limits, are not included.
- The stress is shown as a magnitude: during heating the inner surface is in compression, during cooling in tension.
References
- EN 12952-3 (start-up limits, for context; not applied)
- Quasi-steady heating of a plane wall at a constant rate
- ΔT = Ṫ s²/(2α) (Carslaw and Jaeger); surface stress E β (T_mean − T_s)/(1 − ν) with T_mean − T_s = 2ΔT/3 (Timoshenko)
Questions and answers
Why does thickness matter so much?
ΔT grows with the square of thickness: thick drums must warm slowly.
Is this the code start-up limit?
No: codes combine pressure and thermal stress with fatigue; use this to understand and estimate.
Why quasi-steady?
After an initial transient the profile through the wall settles into a parabola that moves with the ramp.
Method and article reviewed by FireCAD engineering on 13 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.