Worked example
Example: Illustrative 2 kW NiCr element. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Element power | 2.0000 kW |
| Supply voltage | 230.00 V |
| Wire diameter | 0.60000 mm |
| Resistivity at 20 °C | 1.0900 Ω·mm²/m |
| Hot/cold resistance factor at operating temperature | 1.0400 - |
| Wire density | 8,400.0 kg/m³ |
Applying the formula below gives:
| Result | Value |
|---|---|
| Resistance at operating temperature | 26.450 Ω |
| Resistance at 20 °C | 25.433 Ω |
| Wire length | 6.5972 m |
| Surface loading | 16.083 W/cm² |
| Wire mass | 15.669 g |
| Current | 8.6957 A |
Open this example in the calculator and change any input.
Formula
\(R_{hot} = \frac{V^2}{P}, \quad L = \frac{R_{hot}}{C_t}\frac{\pi d^2}{4\rho_{20}}, \quad q = \frac{P}{\pi dL}\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(P\) | Element power | W |
| \(V\) | Supply voltage | V |
| \(d\) | Wire diameter | m |
| \(\rho_{20}\) | Resistivity at 20 °C | Ω·m |
| \(C_t\) | Hot/cold resistance factor at operating temperature | - |
| \(\rho_m\) | Wire density | kg/m³ |
| \(R_{hot}\) | Resistance at operating temperature | Ω |
| \(R_{20}\) | Resistance at 20 °C | Ω |
| \(L\) | Wire length | m |
| \(q\) | Surface loading | W/m² |
| \(m\) | Wire mass | kg |
| \(I\) | Current | A |
Method and standards
Heater wire.
Where it is used
- Designing or rewinding heating elements.
- Checking element surface loading.
Common mistakes
- Ignoring the temperature factor.
- Exceeding the alloy's surface loading.
Assumptions and limits
- Uniform wire; steady operating temperature.
References
- Resistance and surface loading of heating elements
Questions and answers
Why is the hot/cold factor needed?
Resistivity rises with temperature; ignoring it gives slightly too much power when the element is hot.
How do I pick the wire diameter?
Choose one that keeps surface loading within the alloy's limit for the application; thicker wire lasts longer.
What do the defaults represent?
An illustrative 2 kW, 230 V element of 0.6 mm NiCr 80/20 wire (1.09 Ω·mm²/m, C_t = 1.04).
Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.
Sources
Hayt and Kemmerly, Engineering Circuit Analysis, 8th ed. (McGraw-Hill, 2012)