Worked example
Example: Illustrative 600 mA/cm2, 100 cells of 200 cm2. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Current density | 600.00 mA/cm² |
| Practical open-circuit constant | 1.0200 V |
| Area-specific resistance | 0.20000 Ω·cm² |
| Tafel slope constant | 0.035000 V |
| Mass-transport constant | 3.0000e-05 V |
| Mass-transport exponent (cm² per mA) | 0.007500 - |
| Cells in the stack | 100.00 - |
| Active area per cell | 200.00 cm² |
| Fuel utilisation | 95.000 % |
Applying the formula below gives:
| Result | Value |
|---|---|
| Cell voltage | 0.67341 V |
| Power density | 404.04 mW/cm² |
| Ohmic loss | 120.00 mV |
| Activation loss A ln i | 223.89 mV |
| Mass-transport loss | 2.7005 mV |
| Stack voltage | 67.341 V |
| Stack current | 120.00 A |
| Stack power | 8.0809 kW |
| Efficiency on the higher heating value | 43.195 % |
| Efficiency on the lower heating value | 51.052 % |
Open this example in the calculator and change any input.
Formula
\(V = E_{oc} - ir - A\ln i - me^{ni}, \quad \eta_{HHV} = \mu_f\frac{V}{1.481}\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(i\) | Current density | A/m² |
| \(E_{oc}\) | Practical open-circuit constant | V |
| \(r\) | Area-specific resistance | Ω·m² |
| \(A\) | Tafel slope constant | V |
| \(m\) | Mass-transport constant | V |
| \(n\) | Mass-transport exponent (cm² per mA) | - |
| \(N\) | Cells in the stack | - |
| \(A_c\) | Active area per cell | m² |
| \(\mu_f\) | Fuel utilisation | - |
| \(V_c\) | Cell voltage | V |
| \(P/A\) | Power density | W/m² |
| \(\Delta V_{ohm}\) | Ohmic loss | V |
| \(\Delta V_{act}\) | Activation loss A ln i | V |
| \(\Delta V_{trans}\) | Mass-transport loss | V |
| \(V_{stack}\) | Stack voltage | V |
| \(I\) | Stack current | A |
| \(P\) | Stack power | W |
| \(\eta_{HHV}\) | Efficiency on the higher heating value | - |
| \(\eta_{LHV}\) | Efficiency on the lower heating value | - |
Method and standards
Empirical polarisation model.
Where it is used
- Fuel cell stack sizing and operating point selection.
- Fitting test data and comparing cells.
Common mistakes
- Using A/m² inside the logarithm (the constants are for mA/cm²).
- Quoting efficiency without saying HHV or LHV.
Assumptions and limits
- Steady state; constants from a fit to the cell in question.
References
- Empirical polarisation equation V = E_oc − ir − A ln i − m exp(ni)
Questions and answers
Where do the losses come from?
Activation (slow electrode reactions) dominates at low current, resistance in the middle and mass transport (gas supply, water flooding) near the limiting current.
What efficiency does a PEM stack reach?
At 0.65–0.70 V per cell, about 44–47 % on the higher heating value or 52–56 % on the lower; it rises at part load as voltage increases.
What do the defaults represent?
Illustrative PEM constants (E_oc 1.02 V, 0.2 Ω·cm², A 0.035 V, m 3 × 10⁻⁵ V, n 0.0075 cm²/mA) at 600 mA/cm² for 100 cells of 200 cm².
Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.
Sources
Larminie and Dicks, Fuel Cell Systems Explained, 2nd ed. (Wiley, 2003), ch. 3