Worked example
Example: Illustrative hot steel pipe. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Calibration block thickness | 20.000 mm |
| Round-trip time in the block | 6.7800 µs |
| Round-trip time on the part | 3.0500 µs |
| Velocity temperature coefficient | -1.0000e-04 - |
| Part temperature above calibration | 150.00 K |
| Nominal wall thickness | 10.200 mm |
Applying the formula below gives:
| Result | Value |
|---|---|
| Calibrated sound velocity | 5,899.7 m/s |
| Thickness without temperature correction | 8.9971 mm |
| Thickness corrected for temperature | 8.8621 mm |
| Wall loss | 1.3379 mm |
| Wall loss share | 13.117 % |
Open this example in the calculator and change any input.
Formula
\(v = \frac{2t_{ref}}{\Delta t_{ref}}, \quad t = \frac{v\Delta t}{2}(1 + k_T\Delta T)\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(t_{ref}\) | Calibration block thickness | m |
| \(\Delta t_{ref}\) | Round-trip time in the block | s |
| \(\Delta t\) | Round-trip time on the part | s |
| \(k_T\) | Velocity temperature coefficient | - |
| \(T - T_{cal}\) | Part temperature above calibration | K |
| \(t_n\) | Nominal wall thickness | m |
| \(v\) | Calibrated sound velocity | m/s |
| \(t_{uncorr}\) | Thickness without temperature correction | m |
| \(t\) | Thickness corrected for temperature | m |
| \(t_n - t\) | Wall loss | m |
| \((t_n - t)/t_n\) | Wall loss share | - |
Method and standards
UT thickness.
Where it is used
- Corrosion monitoring of pipes and vessels.
- Remaining-life inspection.
Common mistakes
- Calibrating on a different alloy.
- Ignoring temperature on hot lines.
Assumptions and limits
- Longitudinal waves; parallel surfaces; linear velocity–temperature relation.
References
- Pulse-echo thickness measurement
Questions and answers
Why calibrate on a block?
Sound velocity varies with alloy and heat treatment; a known block of the same material sets it.
Does temperature matter?
Yes: sound slows in hot steel, so a gauge calibrated cold reads a hot wall as thicker than it is unless corrected.
What do the defaults represent?
An illustrative steel check: 20 mm block at 6.78 µs, part at 3.05 µs and 150 K hotter, nominal 10.2 mm wall.
Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.
Sources
Krautkrämer and Krautkrämer, Ultrasonic Testing of Materials, 4th ed. (Springer, 1990), Lipták (ed.), Instrument Engineers' Handbook, Vol. 1: Process Measurement and Analysis, 4th ed. (CRC Press, 2003)