FireCADCalc

Ladle Desulphurisation: Sulphur Partition and Final Sulphur

Equilibrium sulphur partition from the slag constant K_SA and dissolved aluminium, and the final steel sulphur from a sulphur balance with the slag mass.

Inputs

Examples: 150 t, 1.5 t slag, 0.03 % Al250 t, 3 t slag, 0.05 % Al, high KSA80 t, 1 t slag, 0.01 % Al, weak slag

Accepted: 1 to 6
Accepted: 1E-4 to 0.2 %
Accepted: 1 to 500 t
Accepted: 0.01 to 50 t
Accepted: 1E-4 to 0.1 %
Accepted: 0 to 2 %

Results

Read log K_SA from the slag chart for the CaO/Al₂O₃ ratio, SiO₂ and temperature (about 3.2-4.6 for lime-saturated calcium aluminate slags). Equilibrium is the limit; the stirring time sets how close the ladle gets. Silicon-killed steels cannot be desulphurised this far because their oxygen potential is higher.

Sulphur partition (%S)/[%S]384.37
Final sulphur in steel21.678ppm
Final sulphur in slag0.83322%
Desulphurisation78.322%

Download PDF CSV Link to this result Compare another case

Log in to save calculations to your dashboard.

Worked example

Example: 150 t, 1.5 t slag, 0.03 % Al. The inputs, in the units selected above:

InputValue
log K_SA (from the slag chart)3.6000 -
Dissolved aluminium0.030000 %
Steel mass150.00 t
Slag mass1.5000 t
Initial sulphur in steel0.010000 %
Initial sulphur in slag0.050000 %

Applying the formula below gives:

ResultValue
Sulphur partition (%S)/[%S]384.37
Final sulphur in steel21.678 ppm
Final sulphur in slag0.83322 %
Desulphurisation78.322 %

Open this example in the calculator and change any input.

Formula

\(L_S = \frac{(\%S)}{[\%S]} = K_{SA}[\%Al]^{2/3}, \quad [\%S] = \frac{W[\%S]_0 + W_s(\%S)_0}{W + L_SW_s}\)

Variables

Symbol Meaning SI unit
\(\log K_{SA}\) log K_SA (from the slag chart) -
\([\%Al]\) Dissolved aluminium -
\(W\) Steel mass kg
\(W_s\) Slag mass kg
\([\%S]_0\) Initial sulphur in steel -
\((\%S)_0\) Initial sulphur in slag -
\(L_S\) Sulphur partition (%S)/[%S] -
\([\%S]\) Final sulphur in steel -
\((\%S)\) Final sulphur in slag -
\(\eta_S\) Desulphurisation -

Method and standards

Slag-metal sulphur equilibrium with a sulphur mass balance.

Where it is used

  • Ladle furnace practice for low-sulphur grades.
  • Choosing slag mass.

Common mistakes

  • Entering %Al as a fraction into the power law.
  • Ignoring sulphur carried in from the furnace slag.

Assumptions and limits

  • Equilibrium; CaS saturation not checked.

Questions and answers

Why does aluminium appear?

Aluminium lowers the oxygen potential; with less oxygen the slag can take more sulphur, so the partition grows as [%Al]^⅔.

How do I reach very low sulphur?

Use a lime-saturated, low-SiO₂ calcium aluminate slag, keep FeO and MnO low, deoxidise well with aluminium and stir hard with argon.

What do the defaults represent?

log K_SA = 3.6, 0.03 % Al, 150 t of steel with 100 ppm S and 1.5 t of slag carrying 0.05 % S: partition 384, final sulphur 22 ppm, 78 % removal.

Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.

Sources

Fruehan (ed.), The Making, Shaping and Treating of Steel, 11th ed., Steelmaking and Refining Volume (AISE Steel Foundation, 1998), sec. 2.10.2, eqs. 2.10.13-2.10.15 and Fig. 2.133

Related calculators

Free engineering calculators: every page computes in SI and converts to your units. Results are for engineering estimation; verify critical designs against the referenced standards.

Rejoining the server...

Rejoin failed... trying again in seconds.

Failed to rejoin.
Please retry or reload the page.

The session has been paused by the server.

Failed to resume the session.
Please retry or reload the page.