Nitriding Case Depth and Time at Temperature

Nitrided case depth after a time from a parabolic growth constant, corrected for temperature by an activation energy, and the time for a target depth.

Inputs

Examples: Illustrative 530 C for 40 h510 C for 60 hPlasma 560 C, 20 h

Accepted: 0.005 to 1
Accepted: 426.85 to 626.85 °C
Accepted: 20 to 400 kJ/mol
Accepted: 426.85 to 626.85 °C
Accepted: 1 to 2,777.8 h
Accepted: 0.01 to 3 mm

Results

Diffusion-controlled growth d = k√t; k² follows Arrhenius, so k scales with exp(−Q/2R·(1/T − 1/T_ref)). Fit k_ref from your own process (gas, salt bath or plasma) and steel; the default is illustrative only.

Growth constant at process temperature (mm/√h)0.091487
Case depth after the time0.57862mm
Time for the target depth29.869h

Download PDF CSV Link to this result Compare another case

Log in to save calculations to your dashboard.

Worked example

Example: Illustrative 530 C for 40 h. The inputs, in the units selected above:

InputValue
Case growth constant at the reference temperature (mm/√h)0.070000 -
Reference temperature510.00 °C
Activation energy140.00 kJ/mol
Process temperature530.00 °C
Nitriding time40.000 h
Target case depth0.50000 mm

Applying the formula below gives:

ResultValue
Growth constant at process temperature (mm/√h)0.091487
Case depth after the time0.57862 mm
Time for the target depth29.869 h

Open this example in the calculator and change any input.

Formula

\(d = k\sqrt t, \quad k = k_{ref}\exp\left[-\frac{Q}{2R}\left(\frac1T - \frac1{T_{ref}}\right)\right]\)

Variables

Symbol Meaning SI unit
\(k_{ref}\) Case growth constant at the reference temperature (mm/√h) -
\(T_{ref}\) Reference temperature K
\(Q\) Activation energy J/mol
\(T\) Process temperature K
\(t\) Nitriding time s
\(d_t\) Target case depth m
\(k\) Growth constant at process temperature (mm/√h) -
\(d\) Case depth after the time m
\(t_t\) Time for the target depth s

Method and standards

Parabolic growth.

Where it is used

  • Nitriding cycle planning.
  • Comparing process temperatures.

Common mistakes

  • Using carburising constants for nitriding.
  • Expecting linear growth with time.

Assumptions and limits

  • Diffusion-controlled growth.

References

  • Parabolic case growth with Arrhenius temperature dependence

Questions and answers

Why does nitriding take so long?

It runs at 500–550 °C, well below carburising temperatures, so nitrogen diffuses slowly; 0.5 mm cases often take 40–80 hours.

Why not just raise the temperature?

Higher temperature speeds diffusion but softens the core and coarsens nitrides, lowering surface hardness.

What do the defaults represent?

An illustrative gas nitriding constant of 0.07 mm/√h at 510 °C, run at 530 °C for 40 hours, target 0.5 mm.

Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.

Sources

Callister and Rethwisch, Materials Science and Engineering, 9th ed. (Wiley, 2014), ch. 5

Related calculators

Free engineering calculators: every page computes in SI and converts to your units. Results are for engineering estimation; verify critical designs against the referenced standards.

Rejoining the server...

Rejoin failed... trying again in seconds.

Failed to rejoin.
Please retry or reload the page.

The session has been paused by the server.

Failed to resume the session.
Please retry or reload the page.