Homogenisation Annealing Time for Dendritic Segregation

Annealing time to reduce dendritic segregation to a target fraction of its amplitude, from dendrite arm spacing and an Arrhenius diffusivity.

Thermal power plantProcess steam and utilitiesRefinery and petrochemical

Inputs

Examples: Illustrative 100 um spacing at 1200 CAluminium billet Mg at 550 CFine 20 um spacing at 1100 C

Accepted: 1 to 10,000 µm
Accepted: 1E-6 to 100 cm²/s
Accepted: 50 to 500 kJ/mol
Accepted: 226.85 to 1,526.8 °C
Accepted: 0.01 to 99 %

Results

A sinusoidal concentration profile of wavelength λ decays as e^(−t/τ), τ = λ²/(4π²D) (Fick's second law). Halving the arm spacing (faster solidification) cuts the time fourfold. Substitutional elements such as Mn, Cr and Ni diffuse slowly in austenite, so full homogenisation of coarse castings is rarely practical.

Diffusivity at temperature4.2727e-10cm²/s
Relaxation time1.6468h
Annealing time7.5837h

Download PDF CSV Link to this result Compare another case

Log in to save calculations to your dashboard.

Worked example

Example: Illustrative 100 um spacing at 1200 C. The inputs, in the units selected above:

InputValue
Dendrite arm spacing (segregation wavelength)100.00 µm
Diffusivity pre-exponential1.6000 cm²/s
Activation energy270.00 kJ/mol
Annealing temperature1,200.0 °C
Residual segregation fraction1.0000 %

Applying the formula below gives:

ResultValue
Diffusivity at temperature4.2727e-10 cm²/s
Relaxation time1.6468 h
Annealing time7.5837 h

Open this example in the calculator and change any input.

Formula

\(\frac{\beta}{\beta_0} = e^{-t/\tau}, \quad \tau = \frac{\lambda^2}{4\pi^2D}, \quad D = D_0e^{-Q/RT}\)

Variables

Symbol Meaning SI unit
\(\lambda\) Dendrite arm spacing (segregation wavelength) m
\(D_0\) Diffusivity pre-exponential m²/s
\(Q\) Activation energy J/mol
\(T\) Annealing temperature K
\(\beta/\beta_0\) Residual segregation fraction -
\(D\) Diffusivity at temperature m²/s
\(\tau\) Relaxation time s
\(t\) Annealing time s

Method and standards

Homogenisation.

Where it is used

  • Ingot and casting soaking before forging.
  • Aluminium billet homogenisation.

Common mistakes

  • Using carbon diffusivity for alloying elements.
  • Taking the secondary arm spacing from a different section size.

Assumptions and limits

  • Sinusoidal profile; constant D; no second phases.

References

  • Decay of sinusoidal segregation by diffusion

Questions and answers

Why does dendrite arm spacing matter so much?

Diffusion distance scales with the square root of time, so time scales with the square of the spacing.

Which element controls homogenisation of steel?

The slowest-diffusing segregated element, usually a substitutional alloying element such as Mn or Cr, not carbon.

What do the defaults represent?

An illustrative 100 µm arm spacing, a substitutional element with D₀ 1.6 cm²/s and Q 270 kJ/mol, annealed at 1,200 °C to 1 % residual segregation.

Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.

Sources

Porter, Easterling and Sherif, Phase Transformations in Metals and Alloys, 3rd ed. (CRC, 2009)

Related calculators

Free engineering calculators: every page computes in SI and converts to your units. Results are for engineering estimation; verify critical designs against the referenced standards.

Rejoining the server...

Rejoin failed... trying again in seconds.

Failed to rejoin.
Please retry or reload the page.

The session has been paused by the server.

Failed to resume the session.
Please retry or reload the page.