Worked example
Example: Illustrative 5-year-old car. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Calendar fade coefficient (per √year) | 2.0000 % |
| Cycle fade per equivalent full cycle | 20.000 ppm |
| Equivalent full cycles per year | 250.00 - |
| Age (years) | 5.0000 - |
| End-of-life state of health | 70.000 % |
| Range when new | 400.00 km |
Applying the formula below gives:
| Result | Value |
|---|---|
| Calendar loss | 4.4721 % |
| Cycle loss | 2.5000 % |
| State of health | 93.028 % |
| Range now | 372.11 km |
| Years to end of life | 36.000 |
Open this example in the calculator and change any input.
Formula
\(SOH = 1 - a\sqrt t - bN_yt, \quad \sqrt{t_{EOL}} = \frac{-a + \sqrt{a^2 + 4bN_y(1 - SOH_{EOL})}}{2bN_y}\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(a\) | Calendar fade coefficient (per √year) | - |
| \(b\) | Cycle fade per equivalent full cycle | - |
| \(N_y\) | Equivalent full cycles per year | - |
| \(t\) | Age (years) | - |
| \(SOH_{EOL}\) | End-of-life state of health | - |
| \(R_0\) | Range when new | m |
| \(Q_{cal}\) | Calendar loss | - |
| \(Q_{cyc}\) | Cycle loss | - |
| \(SOH\) | State of health | - |
| \(R\) | Range now | m |
| \(t_{EOL}\) | Years to end of life | - |
Method and standards
Capacity fade.
Where it is used
- Fleet battery replacement planning.
- Second-life and warranty assessment.
Common mistakes
- Using coefficients fitted at another temperature.
- Treating the model as valid past the knee of rapid fade.
Assumptions and limits
- Additive calendar and cycle terms; before the ageing knee.
References
- Semi-empirical calendar (√t) and cycle ageing
Questions and answers
Why does calendar fade follow √t?
The solid-electrolyte interphase thickens by diffusion-limited growth, which slows with time.
What is a typical end of life?
Warranties commonly guarantee about 70 % of capacity after 8 years or a mileage limit.
What do the defaults represent?
Illustrative fit: 2 %/√year calendar fade and 20 ppm per full cycle at 250 cycles a year, a 5-year-old car with 400 km new range.
Method and article reviewed by FireCAD engineering on 17 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.
Sources
Schmalstieg et al., A holistic aging model for Li(NiMnCo)O2 based 18650 lithium-ion batteries, J. Power Sources 257, 325 (2014)