Worked example
Example: 100 Ah (20 h) at 10 A, k 1.2. The inputs, in the units selected above:
| Input | Value |
|---|---|
| Rated capacity | 100.00 Ah |
| Rated discharge time (the rate the capacity is quoted at) | 20.000 h |
| Discharge current | 10.000 A |
| Peukert exponent | 1.2000 - |
| Depth of discharge allowed | 100.00 % |
Applying the formula below gives:
| Result | Value |
|---|---|
| Run time to the allowed depth of discharge | 8.7055 h |
| Run time ignoring the Peukert effect | 10.000 h |
| Capacity delivered at this current (to full discharge) | 87.055 Ah |
Open this example in the calculator and change any input.
Formula
\(t = DoD \cdot H \left(\frac{C}{I\, H}\right)^k\)
\(t_0 = DoD \cdot \frac{C}{I}, \qquad C_{eff} = I\, H \left(\frac{C}{I\, H}\right)^k\)
Variables
| Symbol | Meaning | SI unit |
|---|---|---|
| \(C\) | Rated capacity | C |
| \(H\) | Rated discharge time (the rate the capacity is quoted at) | s |
| \(I\) | Discharge current | A |
| \(k\) | Peukert exponent | - |
| \(DoD\) | Depth of discharge allowed | - |
| \(t\) | Run time to the allowed depth of discharge | s |
| \(t_0\) | Run time ignoring the Peukert effect | s |
| \(C_{eff}\) | Capacity delivered at this current (to full discharge) | C |
Method and standards
Peukert's empirical law referred to the rated discharge time.
Where it is used
- UPS and inverter backup estimates.
- Solar battery planning.
Common mistakes
- Using the 20 h capacity at a 1 h rate.
- Applying it to lithium cells.
Assumptions and limits
- Constant current and temperature.
- Below the rated rate (I < C/H) the law extrapolates above the rated capacity; real batteries rarely deliver it.
References
- W. Peukert
- Elektrotechnische Zeitschrift 20 (1897); form t = H (C / (I H))^k
Questions and answers
How long does a 100 Ah (20 h) battery last at 10 A with k = 1.2?
8.7 h, delivering 87 Ah instead of 100.
What exponent should I use?
The maker's; flooded lead–acid is higher than AGM or gel.
Why less than rated?
At high current the plates cannot give up all their charge before the voltage collapses.
Method and article reviewed by FireCAD engineering on 12 November 2026. Every result is checked against an independent calculation on each release: how we verify our calculators.